Application of pre-warm deformation to TRIP-aided steels: a new approach to enhance formability

dc.contributor.authorCivek, Tolgahan
dc.contributor.authorSen, Nuri
dc.contributor.authorElkoca, Oktay
dc.date.accessioned2026-07-01T11:40:05Z
dc.date.available2026-07-01T11:40:05Z
dc.date.issued2025
dc.departmentDüzce Üniversitesi
dc.description.abstractThe enhanced formability of TRIP-aided steels relies on the transformation of retained austenite to martensite in microstructure (TRIP effect) at the deformation stage. However, a TRIP effect which has been completed prematurely or has not been sufficiently activated during deformation can adversely affect formability. Therefore, an austenite-martensite transformation that occurs progressively during deformation is essential for optimizing the formability of TRIP-aided steels. This study introduces a novel approach to enhancing the formability of TRIP-aided steels by taking advantage of the temperature dependency of retained austenite stability. The study aims to improve the formability by initially restricting the austenite-martensite transformation in the steel and exploiting the TRIP effect later during the deformation process. For this purpose, a two-stage deformation process was designed. In the first stage (1), the steel was deformed at elevated temperatures (50 degrees C, 100 degrees C, and 150 degrees C) to three predetermined strain levels (5%, 10%, and 15%), effectively suppressing the austenite-to-martensite transformation. In the second stage (2), the steel was cooled to room temperature (RT) to reactivate the TRIP effect and then deformed until fracture. The purpose of the two-stage deformation process was to use the additional strain hardening effect (through TRIP transformation) at the second stage for further delaying the fracture and thereby improving the formability. The results show significant improvement in total elongation: 6.6% (50 degrees C), 9.9% (100 degrees C), 32.2% (150 degrees C) at 15% pre-warm deformation (PWD) and minimal strength compromise: Only 5.2% reduction in tensile strength at optimal conditions (15% PWD, 150 degrees C).
dc.description.sponsorshipScientific and Technological Research Council of Turkey (TUBITAK) [222M321]; TUBITAK -- This study was supported by The Scientific and Technological Research Council of Turkey (TUBITAK) (Project No: 222M321). The authors would like to thank TUBITAK for the financial support given to the project.
dc.identifier.doi10.1007/s40430-025-05990-3
dc.identifier.issn1678-5878
dc.identifier.issn1806-3691
dc.identifier.issue1
dc.identifier.scopus2-s2.0-105022980603
dc.identifier.scopusqualityQ2
dc.identifier.urihttps://doi.org/10.1007/s40430-025-05990-3
dc.identifier.urihttps://hdl.handle.net/20.500.12684/23634
dc.identifier.volume48
dc.identifier.wosWOS:001622493900018
dc.identifier.wosqualityQ2
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.language.isoen
dc.publisherSpringer Heidelberg
dc.relation.ispartofJournal of the Brazilian Society of Mechanical Sciences and Engineering
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.snmzKA_WOS_20260623
dc.subjectTrip-Aided Dp Steel
dc.subjectTrip Effect
dc.subjectPre-Deformation
dc.subjectWarm Deformation
dc.subjectTensile Test
dc.titleApplication of pre-warm deformation to TRIP-aided steels: a new approach to enhance formability
dc.typeArticle

Dosyalar