Effect of crystalline waterproofing admixture on modulus of elasticity of concrete with different W/C ratios

dc.contributor.authorMoghimi, Saeid
dc.contributor.authorHosseınnezhad, Hojjat
dc.contributor.authorBayram, Mustafa Emir
dc.contributor.authorOrhan, Derviş
dc.contributor.authorGültekin, Adil
dc.contributor.authorRamyar, Kambiz
dc.date.accessioned2026-07-01T11:30:21Z
dc.date.available2026-07-01T11:30:21Z
dc.date.issued2026
dc.departmentDüzce Üniversitesi
dc.description.abstractCrystalline waterproofing admixtures (CWA) are used to reduce permeability and provide self-healing effect. Although previous studies have investigated the effects of crystalline admixtures on strength and durability properties of concrete, the effects of these admixtures on the modulus of elasticity of concretes with different W/C ratios remains an area requiring research. In this study, the effect of self-healing provided by CWA on the permeability and mechanical properties of concrete particularly its modulus of elasticity was investigated. For this purpose, 12 concrete mixtures with three different water-to-cement ratios (0.4, 0.5, and 0.6) and four different CWA dosages (0, 0.5, 0.8, and 1.2% by weight of cement) were designed. Three series of specimens were prepared. While one series was tested at the end of 28-day curing without any additional process, second series was pre-loaded to 65% of its compressive strength to induce damage. The last series, following damage induction, underwent additional water curing for 21 days to assess self-healing capacity. To facilitate the observation of self-healing, pre-loading was applied to induce micro-damage. The results indicated that self-healing occurred in concretes containing CWA, the phenomenon verified through SEM imaging. An examination of modulus of elasticity test results revealed that the reference concretes (produced without CWA inclusion) exhibited no substantial improvements. However, CWA-bearing concretes demonstrated enhanced modulus of elasticity, with optimal CWA dosages determined as 1.2%, 0.8%, and 1.2% for W/C ratios of 0.4, 0.5, and 0.6, respectively. Furthermore, the CWA reduced water absorption and water penetration depth under pressure, while enhancing both splitting tensile and compressive strengths.
dc.identifier.dergipark1777248
dc.identifier.doi10.35860/iarej.1777248
dc.identifier.endpage13
dc.identifier.issn2618-575X
dc.identifier.issue1
dc.identifier.orcid0000-0002-6563-9548
dc.identifier.orcid0000-0002-9846-2435
dc.identifier.orcid0000-0001-8452-3447
dc.identifier.orcid0009-0002-2040-5163
dc.identifier.orcid0000-0002-5267-5312
dc.identifier.orcid0000-0003-2200-2691
dc.identifier.startpage1
dc.identifier.urihttps://doi.org/10.35860/iarej.1777248
dc.identifier.urihttps://hdl.handle.net/20.500.12684/22551
dc.identifier.volume10
dc.language.isoen
dc.publisherCeyhun YILMAZ
dc.relation.ispartofInternational Advanced Researches and Engineering Journal
dc.relation.publicationcategoryMakale - Ulusal Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/openAccess
dc.snmzKA_DergiPark_20260623
dc.subjectCrystalline admixture
dc.subjectModulus of elasticity
dc.subjectSelf-healing
dc.subjectTransport properties
dc.subjectWaterproofing
dc.titleEffect of crystalline waterproofing admixture on modulus of elasticity of concrete with different W/C ratios