Kocakulah, GulsumYildirim, MertKoysal, Oguz2021-12-012021-12-0120200957-45221573-482Xhttps://doi.org/10.1007/s10854-019-02797-6https://hdl.handle.net/20.500.12684/10290This paper is a report on electro-optical and dielectric parameters of Ni(II)Pc (nickel(II) phthalocyanine) and CdSeS/ZnS (cadmium selenide sulfide/zinc sulfide) quantum dot (QD) doped 5CB (4-pentyl-4 '-cyanobiphenyl) nematic liquid crystal (LC) in the dark and under UV illumination condition. Electro-optical and dielectric measurements of the samples were carried out using electro-optical switching and dielectric spectroscopy methods, respectively. Dielectric anisotropy, relaxation frequency, dielectric strength, and threshold voltage values were determined using the experimental data. Investigation of dielectric properties demonstrates that relaxation frequency is decreased because of the dispersal of Ni(II)Pc and CdSeS/ZnS QD under UV exposure. The electro-optical investigation also shows that UV illumination and dispersal of Ni(II)Pc and CdSeS/ZnS QD cause a decrease in threshold voltages. Overall, results indicate that Ni(II)Pc, CdSeS/ZnS QD and UV light enhanced the electro-optical and dielectric properties of 5CB nematic LC.en10.1007/s10854-019-02797-6info:eu-repo/semantics/closedAccessWalled Carbon NanotubesCdse Quantum DotsElectrical-PropertiesOptical-PropertiesPhthalocyanineEnhancementDispersionCompositePhotoluminescenceConductivityEffect of intermolecular charge transfer between Ni(II)Pc and CdSeS/ZnS QD on dielectric relaxation mechanism of 5CB nematic liquid crystals in the presence of UV illuminationArticle313258325902-s2.0-85077599384WOS:000512889300085Q2Q3